3M Scotchkote™ XF 895 Fast Curing Floor Coating

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ XF 895 Fast Curing Floor Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to serviceProduct Features:Combines good application characteristics with excellent adhesion to concreteDesigned for application by brush or rollerSuitable for return to service in 1.5 hrsAlso suitable for use on asphalt floor surfaces in combination with 3M Scotchkote Primer FB 856Information provided by 3M
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Solids Content 100 %
100 %
Thickness 152 - 203 microns
6.00 - 8.00 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 75 - 80
75 - 80
ASTM D2240
Tensile Strength at Break 22.6 MPa
3280 psi
ASTM D638
Elongation at Break 15 - 20 %
15 - 20 %
ASTM D412
Abrasion 78
78
[mg] 1000 cycles
Processing Properties Metric English Comments
Cure Time 45.0 - 60.0 min
0.750 - 1.00 hour
Touch Dry
60.0 - 90.0 min
1.00 - 1.50 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray, Clear