Material Notes:
Extrusion Grade, Heat Stabilized
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 56

@Time 3.00 sec
56

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ISO 527-1/-2
Tensile Stress 11.4 MPa

@Strain 5.00 %
1650 psi

@Strain 5.00 %
ISO 527-1/-2
16.5 MPa

@Strain 10.0 %
2390 psi

@Strain 10.0 %
ISO 527-1/-2
20.9 MPa

@Strain 50.0 %
3030 psi

@Strain 50.0 %
ISO 527-1/-2
22.1 MPa

@Strain 100 %
3210 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 250 %
250 %
ISO 527-1/-2
Tensile Modulus 0.260 GPa
37.7 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3