DSM Akulon® K240-HPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K240-HPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 6.8 %
6.8 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Humidity Absorption; Sim. to ISO 62
High Load Melt Index 48 g/10 min

@Load 21.6 kg,
Temperature 275 °C
48 g/10 min

@Load 47.6 lb,
Temperature 527 °F
Calculated from Volume Flow Rate of 40 cm<sup>3</sup>/10min.; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Blow Molding Yes
Heat stabilized or stable to heat Yes
High impact or impact modified Yes
RSV Formic Acid 4 g/100ml
ISO 307
With Fillers Yes