Material Notes:
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wear resistance and greater toughness. CPM Rex 20 was originally designed to replace M42 in any application where cobalt is undesirable. Due to its unique combination of properties, CPM Rex 20 is used in non-cutting applications such as bearings and in plasticizing components such as screw segments, barrels and non-return valves.The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 8.17 g/cc
0.295 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 262 - 285
262 - 285
Annealed
Hardness, Rockwell C 65.5
65.5
Hardening Temperature- 1150°C; Tempering Temperature- 550°C
67.5
67.5
Hardening Temperature- 1205°C; Tempering Temperature- 550°C
Modulus of Elasticity 235 GPa
34100 ksi
Flexural Strength 3957 MPa
573900 psi
Hardening Temperature- 1150°C, Tempering Temperature- 550°C
4005 MPa
580900 psi
Hardening Temperature- 1190°C, Tempering Temperature- 550°C
Charpy Impact 16.0 J
11.8 ft-lb
Hardening Temperature- 1190°C; Tempering Temperature- 550°C
18.0 J
13.3 ft-lb
Hardening Temperature- 1150°C; Tempering Temperature- 550°C
Thermal Properties Metric English Comments
CTE, linear 10.66 µm/m-°C

@Temperature 20.0 - 94.0 °C
5.922 µin/in-°F

@Temperature 68.0 - 201 °F
11.18 µm/m-°C

@Temperature 20.0 - 205 °C
6.211 µin/in-°F

@Temperature 68.0 - 401 °F
12.24 µm/m-°C

@Temperature 20.0 - 540 °C
6.800 µin/in-°F

@Temperature 68.0 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 1.3 %
1.3 %
Chromium, Cr 3.75 %
3.75 %
Iron, Fe 75.92 %
75.92 %
As Remainder
Molybdenum, Mo 10.5 %
10.5 %
Sulfur, S 0.060 - 0.22 %
0.060 - 0.22 %
Tungsten, W 6.25 %
6.25 %
Vanadium, V 2.0 %
2.0 %
Descriptive Properties Value Comments
Grindability; Metal Removed/Wheel Worn 3.5