Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 16.0 J | 11.8 ft-lb | |
Haynes 625 alloy, plate after 1000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 16.0 J | 11.8 ft-lb | Hardening Temperature- 1190°C; Tempering Temperature- 550°C |
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea.. |
|||
Charpy Impact | 16.0 J | 11.8 ft-lb | Hardening Temperature- 1235°C; Tempering Temperature- 540°C |
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS) CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal.. |
|||
Charpy Impact | 16.0 J @Temperature -73.0 °C |
11.8 ft-lb @Temperature -99.4 °F |
V-notch |
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |