Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.24 µm/m-°C @Temperature 38.0 - 649 °C |
6.800 µin/in-°F @Temperature 100 - 1200 °F |
|
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |
|||
CTE, linear | 12.24 µm/m-°C @Temperature 38.0 - 649 °C |
6.800 µin/in-°F @Temperature 100 - 1200 °F |
|
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |
|||
CTE, linear | 12.24 µm/m-°C @Temperature 20.0 - 540 °C |
6.800 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea.. |