Mechanical Properties Metric English Comments
Modulus of Elasticity 235 GPa
34100 ksi
Crucible Steel CPM® 15V® Tool Steel
CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in..
Modulus of Elasticity 235 GPa
34100 ksi
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea..
Modulus of Elasticity 235 GPa
34100 ksi
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or ..