Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTABLEND PA 4016 GF ABS / Nylon 6 Blend, 8% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer , Nylon , Nylon 6
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTABLEND PA
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTABLEND PA 4016 GF ABS / Nylon 6 Blend, 8% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ISO 2577
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 240 °C
40 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 3.00 GPa
435 ksi
ISO 527
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Thermal Properties Metric English Comments
Vicat Softening Point 135 °C

@Load 5.00 kg
275 °F

@Load 11.0 lb
50°C/hr; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Users viewing this material also viewed the following: