ConocoPhillips C-3 Hydraulic Transmission Fluid, Type C-3

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips C-3 Hydraulic Transmission Fluid, Type C-3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydraulic Transmission Fluid, Type C-3 is a heavy-duty, low viscosity fluid for mobile hydraulic systems, torque converters and automatic transmissions. Use it in Allison powershift transmissions and other transmissions that require an Allison C-3, C-2 or C-1 fluid. Common applications include off-highway construction equipment, haul trucks, motor graders, scrapers, farm tractors, cranes, shovels and rollers. Hydraulic Transmission Fluid, Type C-3 offers excellent rust and corrosion protection and wear control. It resists foaming and circulates well, even in low temperatures.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 32.6 °
32.6 °
Viscosity Measurement 121
121
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 31.2 cSt
31.2 cSt
Kinematic Viscosity at 100°C (212°F) 6.5 cSt
6.5 cSt
ASTM Color 1.5
1.5
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
Flash Point 227 °C
441 °F