Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 31.2 cSt | 31.2 cSt | |
ConocoPhillips C-3 Hydraulic Transmission Fluid, Type C-3 Description: Conoco Hydraulic Transmission Fluid, Type C-3 is a heavy-duty, low viscosity fluid for mobile hydraulic systems, torque converters and automatic transmissions. Use it in Allison powersh.. |