Material Notes:
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are available in UL and non-UL grades. In addition, the engineering-grade thermoplastic elastomers we offer can stand up to the most demanding applications . . . while providing the most desirable performance characteristics at a cost that’s more affordable than “ordinary” elastomers.Typical Applications: Ultra flexible, high-grade jacket for cord set applicationsInformation provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Loss On Ignition 24 %
24 %
ASTM 2863
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
10 sec; ASTM D2240
Tensile Strength, Ultimate 15.2 MPa
2200 psi
ASTM D412
Elongation at Break 320 %
320 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746