Polymer Property : Thermal Conductivity = 10.558 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.5237 W/m-K

@Temperature 1000 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Chosun Refractories HAPT-80S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 1.5237 W/m-K

@Temperature 1000 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 1.5237 W/m-K

@Temperature 500 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 932 °F
Chosun Refractories PTC-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 1.5237 W/m-K

@Temperature 1000 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 1.5237 W/m-K

@Temperature 1000 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Chosun Refractories TPA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).