Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 34.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 29.4 - 34.3 MPa

@Temperature 1000 °C,
Time 10800 sec
4270 - 4980 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1500 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1500 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTC-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 34.3 MPa

@Temperature 1350 °C,
Time 10800 sec
3560 - 4980 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved