Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00981 GPa

@Temperature 110 °C,
Time 86400 sec
1.42 ksi

@Temperature 230 °F,
Time 24.0 hour
0.011772 GPa

@Temperature 1000 °C,
Time 10800 sec
1.7074 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 52.0 MPa

@Temperature 110 °C,
Time 86400 sec
7540 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
66.7 MPa

@Temperature 1000 °C,
Time 10800 sec
9670 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1700 °C
3090 °F
limited
Shrinkage -0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
SiO2 8.0 %
8.0 %
Processing Properties Metric English Comments
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Descriptive Properties Value Comments
Installation Method Vibrating, Casting
Material Required for Estimating(kg/?) 2,900
Water Required for Casting(%) 5.5