Chosun Refractories GUN-80L Light-Weight Gunning Castable

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories GUN-80L Light-Weight Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 2.41e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000349 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0006867 - 0.0014715 GPa

@Temperature 500 °C,
Time 10800 sec
0.09960 - 0.21343 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 1.47 - 2.94 MPa

@Temperature 500 °C,
Time 10800 sec
213 - 427 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
2.94 - 4.41 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 640 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.233 W/m-K

@Temperature 260 °C
1.61 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.3722 W/m-K

@Temperature 540 °C
2.579 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Maximum Service Temperature, Air 800 °C
1470 °F
limited
Shrinkage -0.600 %

@Temperature 500 °C,
Time 10800 sec
-0.600 %

@Temperature 932 °F,
Time 3.00 hour
-0.200 %

@Temperature 110 °C,
Time 86400 sec
-0.200 %

@Temperature 230 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Installation Method Gunning
Main Applications Low Temperature
Material Required for Estimating (kg/?) 1,000
Water Required for Casting(%) Nozzle Mixing
Users viewing this material also viewed the following: