Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 1.47 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.47 MPa

@Temperature 1300 °C
213 psi

@Temperature 2370 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.6 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 1.47 MPa

@Temperature 1300 °C
213 psi

@Temperature 2370 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.7 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 1.47 - 2.94 MPa

@Temperature 800 °C,
Time 10800 sec
213 - 427 psi

@Temperature 1470 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-100L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.94 MPa

@Temperature 1000 °C,
Time 10800 sec
213 - 427 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-110L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.94 MPa

@Temperature 500 °C,
Time 10800 sec
213 - 427 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-80L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 2.45 MPa

@Temperature 1000 °C,
Time 10800 sec
213 - 356 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MIX-2 Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 1.47 - 1.96 MPa

@Temperature 110 °C,
Time 86400 sec
213 - 284 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories MIX-3 Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).