Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0053955 GPa

@Temperature 1000 °C,
Time 10800 sec
0.78256 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.0063765 GPa

@Temperature 110 °C,
Time 86400 sec
0.92485 ksi

@Temperature 230 °F,
Time 24.0 hour
Compressive Strength 24.5 MPa

@Temperature 1000 °C,
Time 10800 sec
3560 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
29.4 MPa

@Temperature 110 °C,
Time 86400 sec
4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1450 °C
2640 °F
limited
Shrinkage -0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
-0.100 %

@Temperature 1350 °C,
Time 10800 sec
-0.100 %

@Temperature 2460 °F,
Time 3.00 hour
Descriptive Properties Value Comments
Chemical Analysis(%),Cr2O2 20
Installation Method Casting, Troweling
Main Applications Chemical Plant
Material Required for Estimating (kg/?) 2,600
Water Required for Casting(%) 11