Modulus of Rupture | 0.0053955 GPa @Temperature 500 °C, Time 10800 sec |
0.78256 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories APC-80G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0053955 GPa @Temperature 1000 °C, Time 10800 sec |
0.78256 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0053955 GPa @Temperature 110 °C, Time 86400 sec |
0.78256 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SS50 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |