Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.005886 GPa @Temperature 500 °C, Time 10800 sec |
0.8537 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories APC-80 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 110 °C, Time 86400 sec |
0.8537 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories BCT-130 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 23.0 °C |
0.8537 ksi @Temperature 73.4 °F |
|
Chosun Refractories CRMG-S02 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 - 0.008829 GPa @Temperature 1000 °C, Time 10800 sec |
0.8537 - 1.281 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 - 0.00981 GPa @Temperature 1350 °C, Time 10800 sec |
0.8537 - 1.42 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 - 0.00981 GPa @Temperature 110 °C, Time 86400 sec |
0.8537 - 1.42 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 110 °C, Time 86400 sec |
0.8537 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories LPCT-16DS Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1000 °C, Time 10800 sec |
0.8537 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SW83 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 110 °C, Time 86400 sec |
0.8537 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories TCH-175SV Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.005886 GPa @Temperature 110 °C, Time 86400 sec |
0.8537 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories TCH-175Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |