Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.005886 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.005886 GPa

@Temperature 500 °C,
Time 10800 sec
0.8537 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories APC-80 Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories BCT-130 Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories BCT-145 Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 23.0 °C
0.8537 ksi

@Temperature 73.4 °F
Chosun Refractories CRMG-S02 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 - 0.008829 GPa

@Temperature 1000 °C,
Time 10800 sec
0.8537 - 1.281 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 - 0.00981 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 - 1.42 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 - 0.00981 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 - 1.42 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories LPCT-16DS Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1000 °C,
Time 10800 sec
0.8537 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SW83 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories TCH-175S Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories TCH-175SV Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 GPa

@Temperature 110 °C,
Time 86400 sec
0.8537 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories TCH-175Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).