China Tungsten YG15 Tungsten Carbide for Dies and Wear Part Making

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG15 Tungsten Carbide for Dies and Wear Part Making.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For drawing of steel bars and pipes at high reduction; and also for upsetting, perforating and stamping tools under higher-stress conditions.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 13.9 - 14.2 g/cc
0.502 - 0.513 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A >= 87
>= 87
Flexural Strength 2060 MPa
299000 psi