Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.9 g/cc | 0.502 lb/in³ | |
Wieland 1401 Wilaform Gold Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu.. |
|||
Density | 13.9 - 14.2 g/cc | 0.502 - 0.513 lb/in³ | |
China Tungsten YG15 Cemented Tungsten Carbide for Mining Purposes Top strength and less wear resistance, for bits of rotary hammer rock drills and heavy rock drills , for hard and very hard rocks.Information provided by China Tungsten |
|||
Density | 13.9 - 14.2 g/cc | 0.502 - 0.513 lb/in³ | |
China Tungsten YG15 Tungsten Carbide for Dies and Wear Part Making For drawing of steel bars and pipes at high reduction; and also for upsetting, perforating and stamping tools under higher-stress conditions.Information provided by China Tungsten |
|||
Density | 13.9 g/cc | 0.502 lb/in³ | |
Acerde Tantalum Carbide Tantalum Carbide key properties: Extremely hard refractory ceramic material. The hardness is only exceeded by diamond, Very High melting point, High DensityTantalum Carbide main applications domains.. |