Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.9 - 14.2 g/cc | 0.502 - 0.513 lb/in³ | |
China Tungsten YG15 Cemented Tungsten Carbide for Mining Purposes Top strength and less wear resistance, for bits of rotary hammer rock drills and heavy rock drills , for hard and very hard rocks.Information provided by China Tungsten |
|||
Density | 13.9 - 14.2 g/cc | 0.502 - 0.513 lb/in³ | |
China Tungsten YG15 Tungsten Carbide for Dies and Wear Part Making For drawing of steel bars and pipes at high reduction; and also for upsetting, perforating and stamping tools under higher-stress conditions.Information provided by China Tungsten |
|||
Density | 13.7 - 14.2 g/cc | 0.495 - 0.513 lb/in³ | |
China Tungsten ZC1 Tungsten Carbide Coated substrate of higher toughness and red hardness, for semi-finishing or finishing of carbon steel and alloy steel, generally for threading toolsInformation provided by China Tungsten |