Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Havoline® TC-W3® Two-Cycle Engine Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Havoline®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Havoline® TC-W3® Two-Cycle Engine Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Havoline Two-Cycle Engine Oil TC-W3 is recommended as a premium lubricant for use in two-stroke engines where the latest TC-W3 or earlier general purpose lubricants are recommended. These applications include outboard engines, snowmobiles, motorcycles, lawn mowers, scooters, golf carts, chain saws, and other equipment. It is well suited for engines using oil injection systems with fuel/oil mixture ratios of up to 150:1. Meets:NMMA TC W3ISO-L EGB (JASO FB)API TCTypical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221896; MSDS Number: 8629
Physical Properties Metric English Comments
API Gravity 31.4 °
31.4 °
Brookfield Viscosity 5500 cP

@Temperature -25.0 °C
5500 cP

@Temperature -13.0 °F
Viscosity Measurement 119
119
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
Kinematic Viscosity at 100°C (212°F) 7.3 cSt
7.3 cSt
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
Flash Point 95.0 °C
203 °F
Chemical Properties Metric English Comments
Total Base Number 3.8
3.8
ASTM D2896
Descriptive Properties Value Comments
Ounces of oil to add 1 to 2
per gallon, 100:1 Ratio
2 to 3
per gallon, 50:1 Ratio
4
per gallon, 32:1 Ratio
5 to 6
per gallon, 24:1 Ratio
8
per gallon, 16:1 Ratio, 1 Gallon
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved