Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 5500 cP | 5500 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 40 PVC PVC Copolymer Dispersion Resin F-40 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-40 has been.. |
|||
Brookfield Viscosity | 5500 cP | 5500 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® NVW PVC PVC Homopolymer Dispersion Resin F-NVW is a high molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisols containing F-NVW exhibit low paste viscosities and.. |
|||
Brookfield Viscosity | 5500 cP @Temperature 25.0 °C |
5500 cP @Temperature 77.0 °F |
|
Loctite® 3493 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 5500 cP @Temperature 25.0 °C |
5500 cP @Temperature 77.0 °F |
|
Loctite® 3494 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 5500 cP | 5500 cP | RVT Spindle #2, 20 RPM, 23°C, 20% T.S. in DMF |
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals.Uses: Hot melt adhesive, synthetic leather and fab.. |
|||
Brookfield Viscosity | 5500 cP | 5500 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 38 PVC PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properti.. |
|||
Brookfield Viscosity | 5500 cP @Temperature -25.0 °C |
5500 cP @Temperature -13.0 °F |
|
ChevronTexaco Havoline® TC-W3® Two-Cycle Engine Oil Havoline Two-Cycle Engine Oil TC-W3 is recommended as a premium lubricant for use in two-stroke engines where the latest TC-W3 or earlier general purpose lubricants are recommended. These applicati.. |
|||
Brookfield Viscosity | 5500 cP @Temperature -25.0 °C |
5500 cP @Temperature -13.0 °F |
|
ChevronTexaco TC-W3 2-Cycle Oil FeaturesChevron 2-Cycle Oil TC-W3 is a high quality two-stoke engine lubricant that delivers excellent performance in water-cooled and air-cooled applications. It is formulated to provide excellent.. |
|||
Brookfield Viscosity | 5500 - 9500 cP | 5500 - 9500 cP | RVF #4 sp @ 20 rpm @ 77°F |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Brookfield Viscosity | 5500 cP @Temperature 191 °C |
5500 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M |
|||
Brookfield Viscosity | 5500 cP | 5500 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® NVA PVC PVC Homopolymer Dispersion Resin F-NVA is a high molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisols containing F-NVA exhibit low paste viscosities and.. |
|||
Brookfield Viscosity | 5500 cP @Temperature 25.0 °C |
5500 cP @Temperature 77.0 °F |
|
Loctite® Nuva-Sil® 5091 High Adhesion Potting Potters and Silicon Light Cure AdhesivesLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and sho.. |