Polymer Property : Kinematic Viscosity at 40°C (104°F) = 46.5 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
ASTM D445
ExxonMobil 417 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
ChevronTexaco Havoline® TC-W3® Two-Cycle Engine Oil
Havoline Two-Cycle Engine Oil TC-W3 is recommended as a premium lubricant for use in two-stroke engines where the latest TC-W3 or earlier general purpose lubricants are recommended. These applicati..
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
ASTM D445
ChevronTexaco TC-W3 2-Cycle Oil
FeaturesChevron 2-Cycle Oil TC-W3 is a high quality two-stoke engine lubricant that delivers excellent performance in water-cooled and air-cooled applications. It is formulated to provide excellent..
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
ASTM D445
ExxonMobil 417 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..