Chevron Phillips Marlex® K607 High Density Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® K607 High Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to 1.5 inches thick, separator panels.Processing Recommendations:Extrusion Melt Temperature: Upper Limit: 232°C, Lower Limit: 193°CSpecification Data: ASTM D4976-95 - PE244Data provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 15 hour
15 hour
Condition A, F<sub>50</sub> (100% Igepal CO-630), ASTM D1693
Melt Flow 0.65 g/10 min
0.65 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
2 in per min; ASTM D638 Type IV
Elongation at Break >= 300 %
>= 300 %
2 in per min; ASTM D638 Type IV
Flexural Modulus 1.654 GPa
239.9 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 193 - 232 °C
379 - 450 °F
Extrusion