Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This hexene copolymer is tailored for injection molded applications that require:Excellent flowModerate impact strengthGood stiffnessTypical injection molded applications for 9035 include items such as:Thin wall food containersToysThis resin meets these specifications:ASTM D4976 - PE 231FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ASTM D1505
ESCR 100% Igepal® <= 10 hour
<= 10 hour
Condition B, F50; ASTM D1693
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break <= 100 %
<= 100 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.979 GPa
142 ksi
Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, Type I Specimen; ASTM D746
Users viewing this material also viewed the following: