Chesterton 278 Super Solv

Category Fluid
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 278 Super Solv.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 278 Super Solv is the strongest based cleaner in the Chesterton line. It is designed for those applications where only chlorinated solvents or aromatics previously worked. It will remove most adhesives, epoxies, resins, and tars. Chesterton 278 Super Solv will even attack baked on gums and polymers. Chesterton 278 Super Solv was formulated with the dual goals of strength and safety. This is evidence by several of the products’ features: 1) A flash point of 107°C (225°F). Risk of flammability when using Chesterton 278 Super Solv is considerably minimized. 2) No Chlorinated solvents – no ozone depleting potential and none of the health risks associated with such solvents. 3) Low aromatic content – the raw materials used in 278 Super Solv are non naphthenic but rather based on the synergistic cleaning effect of several polar and non-polar solvents. Chesterton 278 Super Solv can be used in the plant with confidence that virtually all the most difficult industrial soils will be attacked. Yet work safety and the environment will not be compromised. Features:Low Aromatic ContentLow Evaporation RateSafe For Use On All MetalsDissolves Resins, Viscous Polymeric Materials, Epoxies, AdhesivesContains No Ozone Depleting Substance. Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Volatiles 100 %
100 %
Thermal Properties Metric English Comments
Flash Point 107 °C
225 °F
Pensky Martens; ASTM D93-85, DIN 51 755
Descriptive Properties Value Comments
Appearance Clear, transparent liquid
Aromatic Content <0.5%
(C8+)