Cheng Yu Plastic C1100 PC/ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic C1100 PC/ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Index of Compound 16 g/10 min
16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Yield 55.9 MPa
8110 psi
ASTM D638
Flexural Yield Strength 94.1 MPa
13700 psi
ASTM D790
Izod Impact, Notched 49.0 J/cm
91.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 HB
HB