Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 230 °C |
16 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs N30 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP CIP16020FCS Polypropylene, Fast Cycle Information provided by Polykemi AB |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Melt Index of Compound | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC TS16020 LE Polypropylene Copolymer, Mineral Reinforced, Low Emission Information provided by Polykemi AB |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2R PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Melt Index of Compound | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE Information provided by Polykemi AB |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Melt Index of Compound | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Meilian Chemical PE12077 WHITE MASTERBATCH WHITE PE12077 is a LDPE based masterbatch containing high-quality TiO2 without any addition of filler or fluorescence whitener. It is designed for use in economy films for general purpose, especiall.. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 320 °C |
16 g/10 min @Load 11.0 lb, Temperature 608 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 220 °C |
16 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 280 °C |
16 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 340 °C |
16 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 300 °C |
16 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Melt Index of Compound | 16 g/10 min @Temperature 230 °C |
16 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melt Index of Compound | 16 g/10 min @Temperature 230 °C |
16 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ S3001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melt Index of Compound | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |