Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.5 g/cc | 0.379 lb/in³ | |
Wieland 3005 Wilaform Silver Fine silver. Particularly suitable for minting or technical purposes.Applications: chains, coin/shape, laminar decoration, pipesDental |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
Wieland Simidur KF Plus PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
Williams Advanced Alloys WS302 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONITE® 2140C Copper Tungsten Nickel material For structural rotors.Information provided by CMW Inc. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONIUM 23 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONIUM 43 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONIUM 45 Silver Alloy The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low cont.. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONIUM 46 Silver Alloy The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low cont.. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
CMW® ELKONIUM 63 Silver Alloy ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile volta.. |
|||
Density | 10.5 g/cc | 0.379 lb/in³ | |
Indium Corp. Indalloy 207 Pure Silver Information Provided by Indium Corporation |