Material Notes:
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design considerations for prototype and production thermoform tools. In contrast to sintered materials, the pores do not close off after machining allowing excellent definition and surface quality.METAPHOR®-HD 100 AL is the high density grade of the material that is recommended for use in applications where the surface characteristics of the finished part are critical. HD 100 AL is specially formulated to have a smooth surface yielding better transparency on clear or translucent parts. The material is also recommended for use with acrylics and in twin-sheet applications.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 1.898 g/cc
0.06858 lb/in³
Porosity 16 %
16 %
Total porosity (by volume)
Pore Size 12.7 microns
0.500 mil
Mean pore diameter
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Flexural Strength 43.62 MPa
6327 psi
Flexural Modulus 9.205 GPa
1335 ksi
Impact 11
11
Unspecified Impact Strength Test (kJ/m<sup>2</sup>)
Thermal Properties Metric English Comments
CTE, linear 35.6 µm/m-°C

@Temperature 25.0 - 125 °C
19.8 µin/in-°F

@Temperature 77.0 - 257 °F
Thermal Conductivity 20.5 W/m-K

@Temperature 100 °C
142 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 108 °C
226 °F
Martens Dimensional Stability