Polymer Property : CTE, linear = 19.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 35.6 µm/m-°C

@Temperature 25.0 - 125 °C
19.8 µin/in-°F

@Temperature 77.0 - 257 °F
CMT Materials METAPOR® HD 100 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..