Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 43.62 MPa | 6327 psi | |
CMT Materials METAPOR® HD 100 AL Air Permeable Material METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi.. |