Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 7606 GRAPHITE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7606 GRAPHITE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 1.3 g/10 min
1.3 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 7.45 MPa
>= 1080 psi
ASTM D412
Elongation at Break >= 400 %
>= 400 %
ASTM D412
Tear Strength >= 38.53 kN/m
>= 219.9 pli
ASTM D624
Users viewing this material also viewed the following: