Buckeye Polymers BP ABS 3333 R BLK ABS Polymer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP ABS 3333 R BLK ABS Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Our BP ABS 3333 R BLK offers better than average impact while providing good melt flow characteristics in an affordably priced material.Product Features:Good impact and melt flowCan be packaged in new plain white containers or shipped in bulkA balance mixture or recycled content and virgin resins to achieve optimal physical property performance yet meeting aggressive price points.Appearance: BlackForms: PelletsProcessing Method: Injection MouldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 3.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus >= 2.275 GPa
>= 330.0 ksi
ASTM D790
Izod Impact, Notched >= 1.60 J/cm
>= 3.00 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color 1.5
^E; Internal Standard