Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a nice surface aspect and being easy to paint. It has been especially developed for the market of ski bindings, but can be advised as well for any part requiring a high rigidity as well as high impact strength. This product is available in natural and black colorsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527 Type 1A
Elongation at Break 3.9 %
3.9 %
ISO 527 Type 1A
Tensile Modulus 8.30 GPa
1200 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %