Braskem CP 241 Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CP 241 Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CP 241 is a high melt flow rate heterophasic copolymer used for general purposes. This product offers excellent processability, easy mould filling, productivity as well as good stiffness/impact strength balance.Applications: Household; thin-walled parts; easy mould filling; twisted closures. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792A
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 68
68
ASTM D785
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.950 GPa
138 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.500 J/cm

@Temperature -20.0 °C
0.937 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Vicat Softening Point 145 °C
293 °F
10 N; ASTM D1525