Esstech X-690-0000 1,9-Nonanediol Diacrylate, C15H24O4

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-690-0000 1,9-Nonanediol Diacrylate, C15H24O4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1, 9 - Nonanediol diarcylate shows excellent flexibility and water resistance upon curing.  It also has good cross-linking capabilities and low shrinkage making it an excellent material for coatings applications. Listed on the Toxic Substance Control Act List. CAS # 107481-28-7.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Molecular Weight 268.353 g/mol
268.353 g/mol