Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem CP 145 Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CP 145 Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Household; thin-walled parts; easy mould filling. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.54 GPa
223 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm

@Temperature -20.0 °C
0.562 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.470 J/cm

@Temperature 23.0 °C
0.881 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Vicat Softening Point 149 °C
300 °F
-1kg; ASTM D1525