Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45 g/10 min | 45 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 8001 High Density Polyethylene Resin Pétromont HDPE 8001 is a high density, homopolymer polyethylene resin produced using the UNIPOL® Process. This high strength resin is intended for extrusion on cast line, where excellent processab.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 190 °C |
45 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 59 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 300 °C |
45 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
IRPC Polimaxx Porene GA400 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical applianceselectrical fansair conditionersfloppy disks |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 300 °C |
45 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 270 °C |
45 g/10 min @Load 11.0 lb, Temperature 518 °F |
ISO 1133-1 |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ISO 1133-1981E |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 266 °C |
45 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Valox® CS860 PBT+PET (Asia Pacific) 30% glass reinforced PBT+PET blend. Color stable, FR. Housewares, appliances; iron skirt, oven trim/panels.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ASA FR1508 UV Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 250 °C |
45 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Melt Flow | >= 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
>= 45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Absolan® 2300 Sparkle SAN Absolac 2300 Sparkle is a good flow gradeInformation provided by Styrolution |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability Highly Filled, Flame Retardant PBT/PC Alloy, for Injection Molding of "Ceramic Effect" PartsApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacture.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BorPURE™ RJ377MO Polypropylene, Transparent Random Copolymer BorPure™ RJ377MO is a specially modified high MFR transparent polypropylene random copolymer based on proprietary Borealis Nucleation Technology (BNT), with an excellent organoleptic performance. N.. |
|||
Melt Flow | 45 - 65 g/10 min @Load 8.70 kg, Temperature 190 °C |
45 - 65 g/10 min @Load 19.2 lb, Temperature 374 °F |
|
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av.. |
|||
Melt Flow | 45 - 65 g/10 min @Load 8.70 kg, Temperature 190 °C |
45 - 65 g/10 min @Load 19.2 lb, Temperature 374 °F |
|
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 330 °C |
45 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 160 °C |
45 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1260 A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil SFT325 Polypropylene Homopolymer Product Description: A premium homopolymer resin designed to provide soft cotton-like feel and robust spinning to nonwovens applications where fluid barrier is desired.Availability: North America F.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 275 °C |
45 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 260 °C |
45 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade (PBT+X)-MD40Information provided by BARLOG plastics GmbH. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 117 Injection Molding Polypropylene Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 250 °C |
45 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
Polyram RamSter PF201 PBT, General Purpose, Medium Viscosity General purpose, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |