Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Tensile Strength | 35.2 MPa | 5100 psi | 2 in/min; ASTM D638 |
Braskem 52T30V Homopolymer Polypropylene Description: Clarified, Excellent Mold Release, Excellent Flow CharacteristicsApplications: Suggested Uses Include Housewares, Storage Boxes, Containers, VialsInformation provided by Braskem |
|||
Tensile Strength | 35.2 MPa | 5100 psi | 2 in/min; ASTM D638 |
Braskem D180M Homopolymer Polypropylene Description: Low Gas FadeApplications: Suggested Uses Include BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis resin meets the requirements for olefin polym.. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | 2 in/min; ASTM D638 |
Braskem FT021NH Homopolymer Polypropylene Description: High Clarity, Improved AppearanceApplications: Suggested Uses Include Thermoforming, Drink Cups, Deli ContainersThis resin meets the requirements for olefin polymers as defined in 21 CF.. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPP C 200-2 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | 2 in/min; ASTM D638 |
Braskem D180A2 Homopolymer Polypropylene Description: Excellent Melt StabilityApplications: Suggested Uses Include Caps and Closures, Housewares, BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis re.. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk .. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPS HI-100-4 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |