Borealis Borecene Compact™ RM8346RC Black Linear Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Borealis
Trade Name Borecene Compact™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borecene Compact™ RM8346RC Black Linear Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borecene Compact RM8346RC is a third generation linear medium density black polyethylene for rotational molding. Borecene RM8346RC is a special grade, which has passed rigorous tests and can be considered as a possible replacement for crosslinkable polyethylene in many applications. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM8346RC is a black version of Borecene RM8346RC, suitable for fuel tanks. Borecene Compact RM8346 is delivered as new technology powder.Borecene Compact RM8346RC contains 1.0% Carbon Black, which is compounded into the polymer. In addition the grade contains an UV stabilizer which gives excellent UV-stability. The polymer contains long-term antioxidant.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
Base Resin; ASTM D1505
ESCR 10% Igepal® >= 200 hour
>= 200 hour
ARM Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
At 50 mm/min; ASTM D683 IV
Flexural Modulus 0.558 GPa
81.0 ksi
At 2 mm/min; ASTM D790
Dart Drop Total Energy 200.0 J/cm
0.3746 ft-lb/mil
(-4oF/-20°C); ASTM D3763
Dart Drop 152 g/micron
3860 g/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746