Material Notes:
Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toughness and machinability properties.Applications: Heavy-duty machining tools-Not only for the machining of steels but also for nonferrous metals such as nickel-base and titanium alloys. Tools used under extreme compressive stresses-e.g... precision blanking tools for high-strength materials (shaping punches and dies)
Physical Properties Metric English Comments
Density 8.30 g/cc
0.300 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 350
<= 350
Modulus of Elasticity 242 GPa
35100 ksi
Thermal Properties Metric English Comments
CTE, linear 9.60 µm/m-°C

@Temperature 100 °C
5.33 µin/in-°F

@Temperature 212 °F
10.0 µm/m-°C

@Temperature 200 °C
5.56 µin/in-°F

@Temperature 392 °F
10.3 µm/m-°C

@Temperature 300 °C
5.72 µin/in-°F

@Temperature 572 °F
10.6 µm/m-°C

@Temperature 400 °C
5.89 µin/in-°F

@Temperature 752 °F
10.9 µm/m-°C

@Temperature 500 °C
6.06 µin/in-°F

@Temperature 932 °F
11.2 µm/m-°C

@Temperature 600 °C
6.22 µin/in-°F

@Temperature 1110 °F
11.6 µm/m-°C

@Temperature 700 °C
6.44 µin/in-°F

@Temperature 1290 °F
Specific Heat Capacity 0.410 J/g-°C
0.0980 BTU/lb-°F
Thermal Conductivity 19.0 W/m-K
132 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 2.0 %
2.0 %
Chromium, Cr 3.8 %
3.8 %
Cobalt, Co 11 %
11 %
Iron, Fe 60.4 %
60.4 %
As remainder
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 2.5 %
2.5 %
Silicon, Si 0.50 %
0.50 %
Tungsten, W 14.3 %
14.3 %
Vanadium, V 5.1 %
5.1 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000560 ohm-cm
0.0000560 ohm-cm