Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 242 GPa | 35100 ksi | |
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |