Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.9 µm/m-°C @Temperature 21.0 - 93.0 °C |
6.06 µin/in-°F @Temperature 69.8 - 199 °F |
|
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 100 °C |
6.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
Latrobe DuraTechâ„¢ 20CV Powder Metal Stainless Tool Steel DuraTech 20CV is a highly wear resistant, powder metallurgy stainless tool steel. The steel contains a large volume of extremely hard vanadium carbides, which provide excellent wear resistance. Du.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 300 °C |
6.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF14 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 300 °C |
6.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 400 °C |
6.06 µin/in-°F @Temperature 68.0 - 752 °F |
|
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 600 °C |
6.06 µin/in-°F @Temperature 68.0 - 1110 °F |
|
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 500 °C |
6.06 µin/in-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 200 °C |
6.06 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 - 250 °C |
6.06 µin/in-°F @Temperature 68.0 - 482 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |