Material Notes:
BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers excellent processing, stability and clarity for tubing, profile extrusions and some molding applications.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 62 - 68

@Time 10.0 sec
62 - 68

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 15.62 MPa
2266 psi
ASTM D638
Elongation at Break 466 %
466 %
ASTM D638
100% Modulus 0.00547 GPa
0.794 ksi
ASTM D638
Tear Strength 47.0 kN/m
268 pli
ASTM D1004
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
Impact Brittleness; ASTM D746
Clash Berg Stiffness Temperature -59.0 °C
-74.2 °F
135K; ASTM D1043
-41.0 °C
-41.8 °F
35K; ASTM D1043
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Activated Carbon@90°C, % Wt Loss ASTM D1203
Weight Loss (%), ASTM D1239 0.9
Soapy H<sub>2</sub>O Extraction @ 50°C
21.1
Oil Extraction
36
Hexane Extraction