Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00547 GPa | 0.794 ksi | ASTM D638 |
Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers.. |