Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -41.0 °C | -41.8 °F | 35K; ASTM D1043 |
Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers.. |